Chemical Vapour Deposition (CVD)

Three home-built thermal CVD systems allow the growth of crystalline nanostructued metal oxide and metal sulfide thin-films or anisotropic nanostructures (e.g. nanowires) in a temperature window of 200 - 1000 °C.